Customization: | Available |
---|---|
Feature: | Heat Insulation, Water Proof, Fire Proof |
Highest Working Temperature: | 750 |
Still deciding? Get samples of US$ 1/Piece
Order Sample
|
Shipping Cost: | Contact the supplier about freight and estimated delivery time. |
---|
Payment Methods: |
|
---|---|
Support payments in USD |
Secure payments: | Every payment you make on Made-in-China.com is protected by the platform. |
---|
Refund policy: | Claim a refund if your order doesn't ship, is missing, or arrives with product issues. |
---|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Nominal Density(kg)
|
80-120kg
|
Size: L*W(mm)
|
3m*0.6m, 5m*0.6m, 8*1.2m |
Thickness(mm)
|
25-150
|
Item name
|
Test Method
|
Standard Value
|
Test Value
|
|
Thermal conductivity W/(mk)
|
24ºC
|
ASTMC592-16 ASTMC177-19
|
≤0.036
|
0.034
|
93ºC
|
≤0.049
|
0.042
|
||
204ºC
|
≤0.076
|
0.058
|
||
260ºC
|
≤0.092
|
0.070
|
||
371ºC
|
≤0.124
|
0.102
|
||
PH
|
ASTM C795-08
|
<12.5
|
8.4
|
|
Non-Fibrous (Shot)content
|
ASTMC592-16
|
≤25%
|
10%
|
|
w(CI-)%
|
ASTMC795-08 ASTMC871-11
|
When w(SiO32-)+ w(Na+)=0.15%, w(CI-)+w(F-)<0.019%
|
0.0004
|
|
w(F-)%
|
0.0045
|
|||
w(SiO32-)%
|
0.14
|
|||
w(Na+)%
|
0.0071
|
|||
Maximum Flame Spread Index
|
ASTM E84-18
|
≤25
|
0
|
|
Maximum Smoke-developed Index
|
ASTM E84-18
|
≤50
|
0
|
|
Water Vapor Sorption by Weight
|
ASTMC592-16
|
≤5.0%
|
1.4%
|
|
Linear Shrinkage
|
ASTMC592-16
|
≤4.0%
|
2.28%
|
|
Resistance to Fungi
|
ASTM C592-16 ASTMC1338
|
Growth no greater than that a comparative item
|
No growth apparent under 40 Times magnification
|
|
Service Termperature
|
ASTMC592-16
|
No warping, flaming, glowing,Smoldering and smoking
|
650ºC
|
|
Maximum Service Temperature
|
ASTMC447
|
|
750ºC
|
|
Corrosiveness to Steel
|
ASTM C592-16 ASTM C665-17
|
>21
|
35
|
|
Corrosiveness to Aluminum
|
27.5
|
|||
Corrosiveness to Copper
|
24.5
|
|||
Non-combustibility
|
ASTM E136-16a
|
The recorded temperature rise shall not exceed more than 30°C with no flaming and weight loss exceeding 5%
|
non-combustibility
|
|
Odor Emission
|
ASTMC592-16
|
A detectable odor of objectionable nature recorded by more than two of the five panel members shall constitute rejection of the
material. |
None of 5 members considered the odor was objectionable and strong
|